Add to Cart
ASME SA213 TP310S Stainless Steel Tubes For High-Temperature And High-Pressure Superheaters and Reheaters
1. Description
SA213 TP310S stainless steel is austenitic chromium nickel stainless steel. It has good oxidation resistance and corrosion resistance. Because of the high percentage of chromium and nickel, it can work continuously at high temperature and has good high temperature resistance. When the temperature exceeds 800, it begins to soften, and the maximum service temperature is 1200 ℃. Because of the high content of nickel (Ni) and chromium (Cr), A213 TP310S seamless steel pipe has good oxidation resistance, corrosion resistance, acid and alkali resistance and high temperature resistance. It is specially used for manufacturing electric furnace tube and other high temperature occasions.
SA213 TP310S stainless steel seamless steel pipe , the surface can be spray marked, the two ends can be threaded, chamfered, and the two ends of the steel pipe can be protected with a cap protector. A variety of export packaging methods to ensure the safe transportation of products. Our stainless steel seamless steel pipe products are of good quality and many kinds of materials meet the different needs of customers. The products are sold well all over the world, and are widely used in many fields.
2. Chemical composition
Element List | ||||||||||
America standard | European standard | C % max | Mn % max | P % max | S % max | Si % max | Cr % | Ni % | Mo% | Others |
TP304 | 1.4301 | 0.080 | 2.0 | 0.045 | 0.03 | 1.00 | 18.00-20.00 | 8.00-11.00 | - | - |
TP304L | 1.4307 | 0.035 | 2.0 | 0.045 | 0.03 | 1.00 | 18.00-20.00 | 8.00-12.00 | - | - |
TP304H | / | 0.04-0.10 | 2.0 | 0.045 | 0.03 | 1.00 | 18.00-20.00 | 8.00-11.00 | - | - |
TP310S | 1.4845 | 0.080 | 2.0 | 0.045 | 0.03 | 1.00 | 24.00-26.00 | 19.00-22.00 | - | - |
TP316 | 1.4401 | 0.080 | 2.0 | 0.045 | 0.03 | 1.00 | 16.00-18.00 | 11.00-14.00 | 2.00-3.00 | - |
TP316L | 1.4404 | 0.035 | 2.0 | 0.045 | 0.03 | 1.00 | 16.00-18.00 | 10.00-14.00 | 2.00-3.00 | - |
TP316Ti | 1.4571 | 0.080 | 2.0 | 0.045 | 0.03 | 0.75 | 16.00-18.00 | 10.00-14.00 | 2.00-3.00 | Ti:5X(C+N)-0.70 |
TP317 | / | 0.080 | 2.0 | 0.045 | 0.03 | 1.00 | 18.00-20.00 | 11.00-15.00 | 3.00-4.00 | - |
TP317L | 1.4438 | 0.035 | 2.0 | 0.045 | 0.03 | 1.00 | 18.00-20.00 | 11.00-15.00 | 3.00-4.00 | - |
TP321 | 1.4541 | 0.080 | 2.0 | 0.045 | 0.03 | 1.00 | 17.00-19.00 | 9.00-12.00 | - | Ti:5X(C+N)-0.70 |
TP321H | / | 0.04-0.10 | 2.0 | 0.045 | 0.03 | 1.00 | 17.00-19.00 | 9.00-12.00 | - | Ti:4X(C+N)-0.70 |
TP347 | 1.4550 | 0.080 | 2.0 | 0.045 | 0.03 | 1.00 | 17.00-19.00 | 9.00-13.00 | - | Nb:10XC-1.1 |
TP347H | / | 0.04-0.10 | 2.0 | 0.045 | 0.03 | 1.00 | 17.00-19.00 | 9.00-13.00 | - | Nb:8XC-1.1 |
904L | 1.4539 | 0.020 | 2.0 | 0.045 | 0.03 | 1.00 | 19.00-23.00 | 23.00-28.00 | 4.00-5.00 | N:0.10 max/Cu:1.0-2.0 |
S31803 | 1.4462 | 0.030 | 2.0 | 0.045 | 0.03 | 1.00 | 21.00-23.00 | 4.50-6.50 | 2.50-3.50 | N:0.08-0.20 |
S32205 | / | 0.030 | 2.0 | 0.045 | 0.03 | 1.00 | 22.00-23.00 | 4.50-6.50 | 3.00-3.50 | N:0.14-0.20 |
S32750 | 1.4410 | 0.030 | 2.0 | 0.045 | 0.03 | 1.00 | 24.00-26.00 | 6.00-8.00 | 3.00-5.00 | N:0.24-0.32 |
3. Physical Properties
Grade of steel | |||||
China(GB) | China(GB) | America AISI(ASTM) | JIS | (Germany) | |
Old Grade | New Grade | (Japan) | DIN17006 | DIN17007 | |
Stainless steel seamless pipe | 0Cr18Ni9 | TP304/ 06Cr19Ni10 | 304/S30400 | SUS304 | X5CrNi18-10 |
00Cr19Ni10 | TP304L/ 022Cr19Ni10 | 304L/S30403 | SUS304L | X2CrNi19-11 | |
0Cr25Ni20 | TP310/ 06Cr25Ni20 | 310S/31008 | SUS310S | X12CrNi25-21 | |
0Cr17Ni12Mo2 | TP316/ 06Cr17Ni12Mo2 | 316/S31600 | SUS316 | X5CrNiMo17-12-2 | |
00Cr17Ni14Mo2 | TP316L/ 022Cr17Ni12Mo2 | 316L/S31603 | SUS316L | X2CrNiMo18-14-3 | |
0Cr19Ni13Mo3 | TP317/ 06Cr19Ni13Mo3 | 317/S31700 | SUS317 | X5CrNiMo11-13-3 | |
00Cr19Ni13Mo3 | TP317L/ 022Cr19Ni13Mo3 | 317L/S31703 | SUS317L | X2CrNiMo18-16-4 | |
0Cr18Ni10Ti | TP321/ 06Cr18Ni11Ti | 321/S32100 | SUS321 | X6CrNiTi18-10 | |
0Cr18Ni11Nb | TP347/ 06Cr18Ni11Nb | 347/S34700 | SUS347 | X12CrNiNb18-10 |